TiO2 powder was synthesized in the following way. At first, a colloidal solution of Ti in distilled water was obtained by PLA using Nd:YAG laser (wavelength of 1064 nm, frequency of 20 Hz, pulse duration of 7 ns). Then the colloidal solution was dried at 60 °C. After that, the powder was annealed at different temperatures.
6th International conference on advanced nanoparticle generation & excitation by lasers in liquids (ANGEL2021), Hefei, China, June 16th-18th, 2021 : program & technical digest. [S. l.], 2021. P. 86