In this paper, we study the possibility of obtaining iron and titanium-vanadium concentrates with highest contents of iron and titanium, respectively, through hydrometallurgical processing of the titanomagnetite ores of the Chineisk deposit. Ammonium fluoride concentration was varied from 0.08 mol/L to 4.2 mol/L with the other fixed parameters. It was shown that optimum ammonium fluoride concentration for leaching the ore is
Перспективы развития фундаментальных наук : сборник научных трудов XV Международной конференции студентов, аспирантов и молодых ученых, 24–27 апреля 2018 г.. Томск, 2018. Т. 2 : Химия. С. 234-236